压变油皮PU皮革
热压变色油皮PU皮革,油皮纹路,热压变色产品,压花时根据压的图案大小调整压花机的压力,温度,时间,反复尝试几次不同的压力,温度时间取最佳效果。参数参考压力1000KG-1200KG,温度140,时间5S DM-12417
Our leather is processed in conformity with REACH regulation.
Embossing Recommendation
When pressing a color-changing product,adjust the pressure,temperature,and the time of the embossing machine according to the size of the embossing pattern,and try several times to get best results.
Embossing data reference
Pressure 1000kg-1200kg
Temperature 140℃± Time 5s±